Silicon Carbon Anode Swelling Percentage and Capacity Decay: A 50-Cycle In-Situ Comparative Study

0
Sign in to vote or save

Silicon-carbon anode swelling: 8.8% vs 11.2% thickness increase at 3 vs 5 wt.% Si over 50 cycles. In-situ SWE data reveals swelling–capacity decay correlation.